A series of heterogeneous latexes having stage ratios of 40:60 between the first and second stage polymers were prepared by emulsion polymerization. The first-stage polymers were non-polar S-BuA with Tgs ranging from + 100 °C to + 20 °C and the second stage polymer was polar MMA–BuA–MAA having a Tg of 20 °C. The latex particle morphologies were studied using TEM and the thermomechanical properties